ʻO Magnesia Dolomite Brick

Hōʻike Pōkole:

Hana ʻia nā pōhaku lepo dolnesite magnesia i ka maʻemaʻe kiʻekiʻe a me ka magnesia nui a me ke one dolomite magnesia sintered a i ʻole ke one dolomite e like me nā mea maka. Wahi a nā ʻano hana ʻokoʻa, koho i ka lakio kūpono o MgO a me CaO, e hoʻohana i ka mea hoʻopaʻa anhydrous, a hana i kahi mahana kūpono. , Ke kiʻina wela kiʻekiʻe.

He kūpaʻa ikaika nā pōhaku lepo Magnesia dolomite i ka hao haʻahaʻa a me ka haʻahaʻa alkalinity e hoʻomaʻemaʻe ana i ka slag ma waho o ka umu ahi, a he mea pono ia e hoʻopau i ka desulfurization a me ka dephosphorization e hoʻoneʻe i nā impurities i ke kila, a loaʻa ka hopena o ka hoʻomaʻemaʻe kila i hoʻoheheʻe ʻia. Hoʻohana ʻia i loko o nā ipu hao kime, he pilina paʻa ko nā bricks magnesia dolomite me ka clinker sima, maʻalahi e kau ʻia i ka umu ahi, a like ka mānoanoa o ka lole.


ʻIke kikoʻī

HANA HUAOLELO

Hoʻopili a hoʻouna hoʻouna

Nā huahana huahana

Wehewehe

Hana ʻia nā pōhaku lepo dolnesite magnesia i ka maʻemaʻe kiʻekiʻe a me ka magnesia nui a me ke one dolomite magnesia sintered a i ʻole ke one dolomite e like me nā mea maka. Wahi a nā ʻano hana ʻokoʻa, koho i ka lakio kūpono o MgO a me CaO, e hoʻohana i ka mea hoʻopaʻa anhydrous, a hana i kahi mahana kūpono. , Ke kiʻina wela kiʻekiʻe.

He kūpaʻa ikaika nā pōhaku lepo Magnesia dolomite i ka hao haʻahaʻa a me ka haʻahaʻa alkalinity e hoʻomaʻemaʻe ana i ka slag ma waho o ka umu ahi, a he mea pono ia e hoʻopau i ka desulfurization a me ka dephosphorization e hoʻoneʻe i nā impurities i ke kila, a loaʻa ka hopena o ka hoʻomaʻemaʻe kila i hoʻoheheʻe ʻia. Hoʻohana ʻia i loko o nā ipu hao kime, he pilina paʻa ko nā bricks magnesia dolomite me ka clinker sima, maʻalahi e kau ʻia i ka umu ahi, a like ka mānoanoa o ka lole.

Hiʻona

Ka ikaika mechanical maikaʻi ma ke ana wela / kūpaʻa kūpilikiʻi maikaʻi maikaʻi

ʻO ke kūpaʻa maikaʻi loa i ka impregnation Nine / Good creep mahana wela / Hiki ke hoʻomaʻemaʻe i ke kila hoʻoheheʻe ʻia

Palapala noi

Kūpono nā brick of dolnesite magnesia no nā umu hoʻoheheʻe kila. ʻO kahi laʻana, hoʻohana ʻia ka lepe o ka pono o ka hoʻomaʻemaʻe ma waho o ka umu ma ke ʻano he huahana ʻē aʻe no nā pōhaku lepo magnesia-chrome. Ke lilo nei kāna laulā noi i nā mea ʻoi aku ka holehole ʻia ma ke ʻano he huahana koho no nā pōhaku lepo magnesia-chrome, a ʻoi aku ka nui a me ka laulā o kāna noi. Hoʻohana ʻia no ka masonry o ka umu AOD, ka umu VOD a me ka ladle.

Nā Hōʻailona Kino a me nā Kino

Brand / Waiwai

MD15

MD20

MD25

MD30

MD40

Ka nui o ka nui (g / cm3)

3.03

3.03

3.03

3.03

3

ʻIke Porosity (%)

13

12

12

13

13

Anuanu e haki ka ikaika (MPa)

80

90

80

80

80

Hoʻololi Linear paʻa (%) @ 1,500 ℃ x 2hrs

-

-0.35

-

-0.61

-

Refractoriness ma lalo o ka hoʻouka (℃) @ 0.2MPa

1700

1700

1700

1700

1700

Ke mele haku mele (%)

MgO

80.3

76.3

70.3

66.3

56.3

CaO

17

21

27

31

41

Al2O3

0.5

0.5

0.5

0.5

0.5

Fe2O3

0.7

0.7

0.7

0.7

0.7

SiO2

1.3

1.3

1.3

1.3

1.2

Hanana Huahana

1.Raw mea e like ai ka mālama ʻana me ke kino a me ka hoʻāʻo kemika.           
2. Ke kāhi a me ka wili ʻana i nā mea maka nui.
3. Wahi a ka ʻikepili ʻikepili mea kūʻai aku i koi ʻia i ka hoʻohuihui ʻana i nā mea maka.
Ke kaomi ʻana a i ʻole ke kāwili ʻana i ka pōhaku ʻōmaʻomaʻo e hilinaʻi ana i nā mea like ʻole a me ke ʻano o nā pōhaku.
4. E hoʻomaloʻo i nā pōhaku lepo ma ka umu mīkini maloʻo.
5. Hoʻokomo i nā pōhaku lepo i loko o ka pā o ke ana i ke ahi e ke ahi kiʻekiʻe aʻe mai 1300-1800 deg.
6. E nānā ka ʻoihana hoʻonohonoho maikaʻi i nā pōhaku uila i hoʻopau ʻole ʻia.

Hāʻawe a me ka hoʻouna

Hoʻopili e like me ka palekana o ka lawe ʻana i ke kai i ka hae
Hoʻouna: hoʻouka ʻana i nā mea ukana i hoʻopau ʻia ma ka hale hana e ka ipu puka toDoor   
Na ke kai i hoʻopau ʻia i ka lāʻau pallet + kāʻei ea + ʻūwī kīwī ea.


  • Kekahi:
  • Aʻe:

  • 1.Raw mea e like ai ka mālama ʻana me ke kino a me ka hoʻāʻo kemika.           
    2. Ke kāhi a me ka wili ʻana i nā mea maka nui.
    3. Wahi a ka ʻikepili ʻikepili mea kūʻai aku i koi ʻia i ka hoʻohuihui ʻana i nā mea maka.
    Ke kaomi ʻana a i ʻole ke kāwili ʻana i ka pōhaku ʻōmaʻomaʻo e hilinaʻi ana i nā mea like ʻole a me ke ʻano o nā pōhaku.
    4. E hoʻomaloʻo i nā pōhaku lepo ma ka umu mīkini maloʻo.
    5. Hoʻokomo i nā pōhaku lepo i loko o ka pā o ke ana i ke ahi e ke ahi kiʻekiʻe aʻe mai 1300-1800 deg.
    6. E nānā ka ʻoihana hoʻonohonoho maikaʻi i nā pōhaku uila i hoʻopau ʻole ʻia.

    Hoʻopili e like me ka palekana o ka lawe ʻana i ke kai i ka hae
    Hoʻouna: hoʻouka ʻana i nā mea ukana i hoʻopau ʻia ma ka hale hana e ka ipu puka toDoor   
    Na ke kai i hoʻopau ʻia i ka lāʻau pallet + kāʻei ea + ʻūwī kīwī ea.